Machine Learning Modeling for Real-Time Melt Pool Monitoring in Laser Powder Bed Fusion Additive Manufacturing: A Hybrid Approach
Researchers developed a hybrid machine learning approach combining EfficientNetB0 feature extraction with Random Forest classification to achieve 94.58% accuracy and sub-millisecond inference for realβ¦